1. Firstly mix the luminous powder with the low-temperature ceramic glaze powder (the luminous powder accounts for 40% by weight) and water in a ratio of 1:0.6 by weight in a ball mill for 20 minutes to form a glaze slurry. , glaze, glaze and other methods, forming a 200-400 micron glaze layer on the white ceramic green body, drying at 800-960 degrees, and quickly burning in 35 to 50 minutes, can be made into luminous interior wall glaze Brick products.
2. The Xingsheng Luminous Powder and the low-temperature ceramic glaze powder are thoroughly mixed uniformly (the luminous powder accounts for 30-40% by weight) and mixed with an appropriate amount of screen printing ink to prepare a slurry for screen printing. A luminous pattern was formed by screen printing a luminous glaze on the white glaze layer of the unburned floor tile (80 to 120 mesh for the screen). On the surface of the pattern, burn a layer of transparent glaze. It is rapidly fired in 35 to 45 minutes at a temperature of 850 to 960 degrees. Can be made into luminous pattern tile products.
3. Firstly mix the prosperous luminous powder with the low-temperature ceramic glaze powder (the luminous powder accounts for 30-40% by weight) and mix with a suitable screen printing ink to prepare a slurry for screen printing. Use a wire mesh on the luminous pattern, stack transparent dry glaze powder, and quickly fire at 40 to 950 degrees for 40 to 50 minutes. A luminous pattern having a convex effect is formed. The luminous pattern interior wall is decorated with glazed tiles.
Second, the attention of Xingsheng luminous powder:
(1) Avoid strong friction between the luminous powder and metal objects, otherwise it will affect the luminous effect. The luminous powder particle size is generally 160 to 300 mesh or 200 to 400 mesh.
(2) If the glaze is settling, add 2 to 4% of the turmeric soil to increase the suspensibility of the glaze slurry.
(3) Select the low temperature glaze matched with the porcelain blank to control the temperature and time. If the temperature is too high, the burn time will affect the brightness.